Keywords
กระเบื้องซีเมนต์ลอนคู่, ใยหิน, โมเม้นต์ดัดแตกหัก, ความต้านแรงแตกหัก, corrugated roofing sheet, asbestos, modulus of rupture, rupture resistance
Abstract
Testing on one sample of asbestos-based and three samples of asbestos-free corrugated roofing tiles disclosed that the water absorption of sample with asbestos was 2.46 per cent and the asbestos-free samples were between 1.59 and 1.71 per cent; for mechanical properties by means of modulus of rupture and rupture resistance for roofi ng sheet sample with asbestos were 80.14 N-m and 35.45 N, respectively, while the modulus of rupture of the three asbestos-free samples was ranged from 83.38 to 86.03 N-m and from 71.45 to 128.18 N for rupture resistance.
Key words: corrugated roofing sheet, asbestos, modulus of rupture, rupture resistance
Recommended Citation
Sirianuntapiboon, Suntud; Rarunroung, Methinee; Asavapisit, Suwimol; and Menasveta, Piamsak.
2011
Property Tests on Cement-based Corrugated Roofi ng Tiles, with and without Asbestos.
Asian Medical Journal and Alternative Medicine. 11,
4 (Oct. 2011 ), 580-587.
Available at: https://doi.org/10.70933/2773-9465.1453
Creative Commons License

This work is licensed under a Creative Commons Attribution-NonCommercial-No Derivative Works 4.0 International License.